I-Dongguan Enuo mold Co., Ltd iyinxalenye yeQela le-Hong Kong BHD, uyilo lokubumba iplastiki kunye nokuvelisa lishishini labo elingundoqo.Ngaphaya koko, iinxalenye zentsimbi ze-CNC machining, iimveliso zeprototype ze-R&D, indawo yokuhlola/iGauji ye-R&D, ukubunjwa kweemveliso zeplastiki, ukutshiza kunye nokuhlanganisa nazo ziyabandakanyeka.

How many do you know about part molding defect -marks
Ukudala 5 Amagqabantshintshi Oct-26-2020

Zingaphi ozaziyo malunga inxalenye yokubumba isiphene -amanqaku

Ngexesha lolingo lokungunda, iziphene zokubumba zikholisa ukwenzeka ngaphandle koqikelelo oluqinisekileyo, kungoko injineli elungileyo yolingo lokungunda kufuneka ibe namava atyebileyo okugweba isizathu ngokukhawuleza kangangoko, njengoko iindleko zinyuka ngexesha elichithwe kumatshini wokutofa.

Apha iqela lethu liqokelele amava athile, ukuba oku kwabelana kungabonisa ingcebiso encinci ukuze kuzuze ukusombulula ingxaki efanayo, siya konwaba kakhulu.

 def

Apha sithetha ngamanqaku amathathu: "Iimpawu ezitshisiweyo", "Amanqaku oMmanzi" kunye "neempawu zomoya".

def2

def

Iimbonakalo:

·Ukuvela rhoqo

·Ukubonakala kwinqanaba elimxinwa elinqamlezayo okanye indawo yomgibe womoya

·Iqondo lobushushu lokunyibilika liphantse libe ngumda ophezulu weqondo lobushushu benaliti

·Isiphene sinomphumo othile ngokunciphisa isantya se-screw press

·Ixesha lePlastiki lide kakhulu, okanye uhlale kwindawo engaphambili yesikrufu sokushicilela ixesha elide

·Imathiriyeli yeplastiki esetyenzisiweyo isetyenziswe ngokugqithisileyo okanye imathiriyeli iye yanyibilika amaxesha amaninzi ngaphambili

·Ukubonakala kubumba kunye nenkqubo yembaleki eshushu

·Ukungunda ngomlomo ovaliweyo (Vala uMlomo)

def4
def5

Iimbonakalo:

·Imathiriyeli ekrwada ineempawu zokufunxa amanzi (ezinje: PA, ABS)
·Ukutofa iplastiki enyibilikisiweyo emoyeni kancinane, amaqamza kunye nesenzeko somphunga siya kuvela
·Imilo yamanqaku aboniswe njengesakhiwo "somngxuma".
·Ukufuma kwezinto phambi kokuba inaliti iphezulu kakhulu
·Isiqulatho sokufuma kokusingqongileyo siphezulu kakhulu (ingakumbi xa umoya udibana nokungunda okubandayo okanye amasuntswana e-colloidal,
·Iphawula imilo njengo “U” imilo, indawo enkulu kwaye akukho migca imhlophe ekhazimlayo
·Amanqaku anemigca arhangqwe yiperimitha erhabaxa

3, Amanqaku omoya

def6

def7

Ngokubanzi, iimilo zeempawu zomoya zirhabaxa, zinombala wesilivere okanye omhlophe, zidla ngokuvela kwindawo engqukuva/egobileyo, iimbambo/ubunzima bodonga butshintsha iindawo okanye kummandla womlomo, isango lokungena lidla ngokubonakala umaleko omncinci wamanqaku omoya;Iimpawu zomoya nazo zibonakala kwikrola, umzekelo: ukukrola umbhalo okanye indawo yokudakumba yendawo.

·Isiphene sincinci ngoxinzelelo olusezantsi
·Xa isikrufu sihamba kancinci, isiphene siba sincinci
·Ibhamuza elibonakalayo ebhiya
·Ipateni yegesi kwizinto ezityhidiweyo yayiyisakhiwo esifana nomngxuma

Ngaphandle kweentlobo ezingentla, sikwanayo "namanqaku e-Glass-fiber" kunye "namanqaku oMbala" kwinqanaba le-surface.so kwixa elizayo, amava amaninzi okubumba aya kukwabelwana ngayo nabahlobo abathandekayo kwi-linkedin, ukuba unezimvo ezahlukeneyo malunga neposi yam, nceda. Ngobubele undazise izimvo zakho, njengoko sisazi, i-linkedin isoloko iliqonga elifanelekileyo lokuba sabelane, sifunde kwaye siphucule!